37机一模6产品稳定参数。刚开始开机将剂量降到8.5开好后送初件,说8号7号模有毛边。后将温度降掉一点,射速提高一点,降到不饱模开机逐步剂量加到7.5后送初件产品OK,生产中包装员说还有不饱模,剂量加到8.0后正常生产。
Disclaimer: The content above represents only the views of the author or guest. It does not represent any views or positions of FOLLOWME and does not mean that FOLLOWME agrees with its statement or description, nor does it constitute any investment advice. For all actions taken by visitors based on information provided by the FOLLOWME community, the community does not assume any form of liability unless otherwise expressly promised in writing.